Long Wear Smooth Foundation

Reference ID

G3052-459.02

Phase Ingredient INCI Name % (wt)
A Gransil EP-9 Polysilicone-11 (and) Water (and) Laureth-12 (and) Phenoxyethanol (and) Ethylhexylglycerin 5.00
Granresin MQI-T50 Isododecane (and) Polymethylsilsesquioxane / Trimethylsiloxysilicate 7.50
Isododecane Isododecane 12.50
Gransurf 67 PEG-10 Dimethicone 2.00
Gransurf 50C-HM Dimethicone (and) PEG/PPG-18/18 Dimethicone 2.00
Euxyl PE 9010 Phenoxyethanol (and) Ethylhexylglycerin 1.00
Bentone 38V Disteardimonium Hectorite 0.60
B Suncroma Yellow Iron Oxide Iron Oxide 1.31
Suncroma Red Iron Oxide Iron Oxide 0.40
Suncroma Black Iron Oxide Iron Oxide 0.13
RBTS-MS3 Titanium Dioxide (CI 77891) (and) Methicone 6.58
Sericite DNN Mica 6.58
Dimethicone, 5cSt Dimethicone 7.50
Gransurf 67 PEG-10 Dimethicone 2.50
C Deionized Water Water 35.40
Glycerin Glycerin 5.00
Butylene Glycol Butylene Glycol 3.00
Sodium Chloride Sodium Chloride 1.00

Procedure

  1. Combine Phase A in the main kettle and homogenize at 1000 to 1500 rpm until uniform.
  2. Combine Phase B and run ball mill until the drawdown passes 10 micron on Hegman Gauge.
  3. Combine Phase C in the support kettle and mix until all solids are dissolved.
  4. Add Phase B into the main kettle while homogenizing and continue mixing for at least 20 minutes.
  5. Add Phase C very slowly to the main kettle while homogenizing. At the end, increase to speed to 1500 to 2500 rpm to finish the batch.