Smooth Foundation

Super smooth foundation featuring Gransil EP-9, Gransurf 67 and Gransurf 50C

Reference ID

G3052-242.02

Database ID

Smooth Foundation

PartIngredientINCI Name% (wt)
A Gransil EP-9 Polysilicone-11 (and) Water (and) Laureth-12 (and) Phenoxyethanol (and) Ethylhexylglycerin5.00
  Dimethicone, 5cStDimethicone20.00
  Gransurf 67 PEG-10 Dimethicone 2.00
  Gransurf 50C Dimethicone (and) PEG/PPG-18/18 Dimethicone 2.00
  Euxyl PE 9010 Phenoxyethanol (and) Ethylhexylglycerin1.00
  Bentone 38V Disteardimonium Hectorite0.60
       
B Suncroma Yellow Iron OxideIron Oxide1.31
  Suncroma Red Iron OxideIron Oxide0.40
  Suncroma Black Iron OxideIron Oxide0.13
  RBTS-MS3Titanium Dioxide (CI 77891) (and) Methicone 6.58
  Sericite DNNMica6.58
  Dimethicone, 5cStDimethicone7.50
  Gransurf 67 PEG-10 Dimethicone 2.50
       
C Deionized WaterWater35.40
  GlycerinGlycerin5.00
  Butylene GlycolButylene Glycol3.00
  Sodium ChlorideSodium Chloride1.00
       
  Total: 100.00

Procedure

1 Combine Phase A in the main kettle and homogenize at 1000-1500 rpm until uniform.
2 Combine Phase B and run ball mill until the drawdown passes 10 micron on Hegman Gauge.
3 Combine Phase C in the support kettle and mix until uniform.
4 Add Phase B into the main kettle while homogenizing, and continue mixing for at least 20 minutes.
5 Add Phase C very slowly to the main kettle while homogenizing. At the end, increase to speed to 1500-2500 to finish the batch.