Extended Wear CC Serum
Reference ID
G103-330.03
Phase | Ingredient | INCI Name | % (wt) |
---|---|---|---|
A | Gransil EP-9 | Polysilicone-11 (and) Water (and) Laureth-12 (and) Phenoxyethanol (and) Ethylhexylglycerin | 5.00 |
Gransurf 67 | PEG-10 Dimethicone | 2.00 | |
Gransurf 50C-HM | Dimethicone (and) PEG/PPG-18/18 Dimethicone | 2.00 | |
Granresin MQC-T50 | Cyclopentasiloxane (and) Polymethylsilsesquioxane / Trimethylsiloxysilicate | 10.00 | |
Dimethicone, 5CST | Dimethicone | 15.00 | |
Bentone 38V | Disteardimonium Hectorite | 0.60 | |
Bentone 38V | Disteardimonium Hectorite | 1.00 | |
B | Dimethicone, 5CST | Dimethicone | 7.50 |
RBTS-MS3 | Titanium Dioxide (CI 77891) (and) Methicone | 6.58 | |
Suncroma Yellow Iron Oxide | Iron Oxide | 1.31 | |
Suncroma Red Iron Oxide | Iron Oxide | 0.40 | |
Suncroma Black Iron Oxide | Iron Oxide | 0.13 | |
Sericite DNN | Mica | 6.58 | |
Gransurf 67 | PEG-10 Dimethicone | 2.50 | |
C | Deionized Water | Water | 30.40 |
Glycerin | Glycerin | 5.00 | |
Butylene Glycol | Butylene Glycol | 3.00 | |
Sodium Chloride | Sodium Chloride | 1.00 |
Procedure
- Combine Phase A in the main kettle and homogenize until uniform.
- Combine Phase B and ball mill until uniform.
- Combine Phase C in the support kettle and mix until uniform.
- Add Phase B into the main kettle while homogenizing. Continue to mix for 20 minutes.
- Slowly add Phase C into the main kettle while homogenizing. Continue to mix for 20 minutes and finish the batch.